Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Laser Welding Characteristic of Dissimilar Metal for Aluminum to Steel
Yong Kim
JWJ. 2017;35(5):16-22.   Published online 2017 October 24    DOI: https://doi.org/10.5781/JWJ.2017.35.5.3

Excel Download

Laser Welding Characteristic of Dissimilar Metal for Aluminum to Steel
Journal of Welding and Joining. 2017;35(5):16-22   Crossref logo
Link1 Link2 Link3

Investigations on Laser Beam Welding of Different Dissimilar Joints of Steel and Aluminum Alloys for Automotive Lightweight Construction
Physics Procedia. 2016;83:383-395   Crossref logo
Link1 Link2

High-power Laser Welding of Thick Steel-aluminum Dissimilar Joints
Physics Procedia. 2016;83:396-405   Crossref logo
Link1 Link2

Dissimilar welding of carbon steel to 5754 aluminum alloy by Nd:YAG pulsed laser
Materials & Design. 2010;31(1):458-465   Crossref logo
Link1 Link2

Dissimilar Aluminum-Steel FSW Lap Joints
Friction Stir Welding and Processing VIII. 2015;137-143   Crossref logo
Link1

Computational Modeling of Dissimilar Metal CO2 Laser Welding: Applied to Copper and 304 Stainless Steel
Procedia Engineering. 2015;127:208-214   Crossref logo
Link1 Link2

Friction Stir Scribe Welding of Dissimilar Aluminum to Steel Lap Joints
Friction Stir Welding and Processing VIII. 2015;163-169   Crossref logo
Link1

Laser lap welding quality of steel/aluminum dissimilar metal joint and its electronic simulations
The International Journal of Advanced Manufacturing Technology. 2016;86(5-8):2231-2242   Crossref logo
Link1 Link2 Link3 Link4

Dissimilar Metal Active Gas Welding of TWIP and DP Steel Sheets
steel research international. 2014;86(5):495-501   Crossref logo
Link1

Influences of TIG welding parameters on tensile behavior of dissimilar metal lap joint for low carbon steel and AA1050
Proceedings of the 1st International Joint Symposium on Joining and Welding. 2013;493-498   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.