Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
The Study on Characteristics of Dissimilar Weld Metals between AA6061-T6 and Silafont-36 by Laser Welding
Jun-Hyeok Hyun, Tae-Woo Shin, Bok-Su Jang, Sang-Ho Kim, Gun-Ho Go, Tae-Young Kim, Jin-Hyun Koh
JWJ. 2017;35(5):71-76.   Published online 2017 October 23    DOI: https://doi.org/10.5781/JWJ.2017.35.5.10

Excel Download

The Study on Characteristics of Dissimilar Weld Metals between AA6061-T6 and Silafont-36 by Laser Welding
Journal of Welding and Joining. 2017;35(5):71-76   Crossref logo
Link1 Link2 Link3

Hybrid laser–arc welding of dissimilar metals
Hybrid Laser-Arc Welding. 2009;270-295   Crossref logo
Link1 Link2 Link3

Friction Stir Welding of Dissimilar Materials Aluminum AL6061-T6 to Ultra Low Carbon Steel
Metals. 2017;7(2):42   Crossref logo
Link1

Effect of rotation speed on friction behavior of rotary friction welding of AA6061-T6 aluminum alloy
Welding in the World. 2018;   Crossref logo
Link1 Link2 Link3

Microstructure and Mechanical Properties of Dissimilar Friction Stir Welding between Ultrafine Grained 1050 and 6061-T6 Aluminum Alloys
Metals. 2016;6(10):249   Crossref logo
Link1

Microstructure and properties of a dissimilar weld between alloy 617 and A387 steel using different filler metals
Welding in the World. 2018;   Crossref logo
Link1 Link2 Link3

Weldability in friction stir welding between dissimilar metals with circular weld line
Proceedings of the 1st International Joint Symposium on Joining and Welding. 2013;203-206   Crossref logo
Link1 Link2

Study on Fiber Laser Welding of AA6061-T6 Samples through Numerical Simulation and Experiments
Procedia Engineering. 2017;174:732-739   Crossref logo
Link1 Link2

Effect of the Welding Speed on the Macrostructure, Microstructure and Mechanical Properties of AA6061-T6 Friction Stir Butt Welds
Metals. 2017;7(2):48   Crossref logo
Link1

Study on weld pool behaviors and ripple formation in dissimilar welding under pulsed laser
Optics & Laser Technology. 2017;93:1-8   Crossref logo
Link1 Link2