Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
MIG Welding Optimization of Muffler Manufacture by Microstructural Change and Thermal Deformation Analysis
Seung Ho Lee, Eok Soo Kim, Jin-Young Park, Jun Choi
JWJ. 2017;35(5):29-37.   Published online 2017 September 27    DOI: https://doi.org/10.5781/JWJ.2017.35.5.5

Excel Download

MIG Welding Optimization of Muffler Manufacture by Microstructural Change and Thermal Deformation Analysis
Journal of Welding and Joining. 2017;35(5):29-37   Crossref logo
Link1 Link2 Link3

Numerical analysis of thermal deformation and residual stress in automotive muffler by MIG welding
Journal of Computational Design and Engineering. 2018;5(4):382-390   Crossref logo
Link1 Link2

MIG welding of stainless steel
Mig Welding Guide. 2006;204-210   Crossref logo
Link1 Link2 Link3

Equipment for MIG welding
Mig Welding Guide. 2006;29-48   Crossref logo
Link1 Link2 Link3

The MIG welding process
Mig Welding Guide. 2006;3-28   Crossref logo
Link1 Link2 Link3

Shielding gases in MIG welding
Mig Welding Guide. 2006;49-70   Crossref logo
Link1 Link2 Link3

Consumables in MIG welding
Mig Welding Guide. 2006;71-79   Crossref logo
Link1 Link2 Link3

Pulsed MIG welding
Mig Welding Guide. 2006;90-97   Crossref logo
Link1 Link2 Link3

Assessing weld quality in MIG welding
Mig Welding Guide. 2006;130-143   Crossref logo
Link1 Link2 Link3

Reducing costs in MIG welding
Mig Welding Guide. 2006;168-176   Crossref logo
Link1 Link2 Link3

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.