Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
The Changes of Chemical Composition and Microstructure in Electroslag Cladding Overlays by using AISI 430 Stainless Steel Strip
Jae-Young Jung, Tae-Kwon Ha
JWJ. 2017;35(5):48-56.   Published online 2017 September 13    DOI: https://doi.org/10.5781/JWJ.2017.35.5.7

Excel Download

The Changes of Chemical Composition and Microstructure in Electroslag Cladding Overlays by using AISI 430 Stainless Steel Strip
Journal of Welding and Joining. 2017;35(5):48-56   Crossref logo
Link1 Link2 Link3

Effects of Welding Parameters on the Overlay Welding Behaviors in Electroslag Cladding by using AISI 430 Stainless Steel Strip - Experimental Study
Journal of Welding and Joining. 2017;35(5):77-86   Crossref logo
Link1 Link2 Link3

Variations of Chemical Composition and Effects of Welding Parameters on the Overlay Welding Behaviors and Fluxes in Electroslag Cladding by using a New 420-series Stainless Steel Strip
Journal of Welding and Joining. 2017;35(6):32-41   Crossref logo
Link1 Link2 Link3

Electroslag and submerged arc stainless steel strip cladding
Anti-Corrosion Methods and Materials. 1998;45(1):41-47   Crossref logo
Link1 Link2

Interface microstructure across cladding of super duplex stainless steel with austenitic stainless steel buffer layer
Surface and Coatings Technology. 2014;259:532-542   Crossref logo
Link1 Link2

Strain aging of AISI 430 ferritic stainless steel
Scripta Materialia. 1997;38(2):185-190   Crossref logo
Link1 Link2

The Effects of Nitrogen Content and Cold Rolling Reduction on the Mechanical Properties of New 420-series Stainless Steel Strip having a Mesh As-Welded Structure by the Electroslag Cladding
Journal of Welding and Joining. 2017;35(6):42-50   Crossref logo
Link1 Link2 Link3

Microstructure, mechanical properties and chemical degradation of brazed AISI 316 stainless steel/alumina systems
Materials Science and Engineering: A. 2008;480(1-2):306-315   Crossref logo
Link1 Link2

Effect of neutron irradiation on the microstructure of the stainless steel electroslag weld overlay cladding of nuclear reactor pressure vessels
Journal of Nuclear Materials. 2013;443(1-3):266-273   Crossref logo
Link1 Link2

GMAW dissimilar welding of AISI 409 ferritic stainless steel to AISI 316L austenitic stainless steel by using AISI 308 filler wire
Engineering Science and Technology, an International Journal. 2017;20(4):1334-1341   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.