Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Laser Cladding with Al-36%Si Powder Paste on A319 Al Alloy Surface to Improve Wear Resistance
Hyoung-Keun Lee
JWJ. 2017;35(2):58-62.   Published online 2017 April 28    DOI: https://doi.org/10.5781/JWJ.2017.35.2.9

Excel Download

Laser Cladding with Al-36%Si Powder Paste on A319 Al Alloy Surface to Improve Wear Resistance
Journal of Welding and Joining. 2017;35(2):58-62   Crossref logo
Link1 Link2 Link3

Laser Cladding by Printing Si Powder Paste on A1050 Al Alloy Surface
Journal of Welding and Joining. 2018;36(1):57-64   Crossref logo
Link1 Link2 Link3

Wear resistance of plasma sprayed Al–Si binary alloy coatings on A6063 Al alloy substrate
Surface and Coatings Technology. 2001;142-144:277-282   Crossref logo
Link1 Link2

Broad-beam laser cladding of Al–Si alloy coating on AZ91HP magnesium alloy
Surface and Coatings Technology. 2006;201(6):2701-2706   Crossref logo
Link1 Link2

Microstructure and corrosion resistance of magnesium alloy ZE41 with laser surface cladding by Al–Si powder
Surface and Coatings Technology. 2008;202(20):4901-4914   Crossref logo
Link1 Link2

Friction and wear behavior of Ti following laser surface alloying with Si, Al and Si+Al
Wear. 2000;242(1-2):18-27   Crossref logo
Link1 Link2

Al 2 O 3 eliminating defects in the Al coating by laser cladding to improve corrosion and wear resistance of Mg alloy
Materials and Corrosion. 2019;71(6):980-991   Crossref logo
Link1 Link2 Link3 Link4

Improving the wear resistance of AZ91D magnesium alloys by laser cladding with Al–Si powders
Materials Letters. 2009;63(1):19-21   Crossref logo
Link1 Link2

Corrosion and wear resistance improvement of magnesium alloys by laser cladding with Al-Si
Physics Procedia. 2011;12:353-363   Crossref logo
Link1 Link2

Effect of humidity on friction and wear of AlSi eutectic alloy and AlSi alloy-graphite composites
Wear. 1996;198(1-2):169-175   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.