Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Experimental Investigation of Laser Spot Welding of Ni and Au-Sn-Ni Alloy
Dongkyoung Lee
JWJ. 2017;35(2):1-5.   Published online 2017 April 28    DOI: https://doi.org/10.5781/JWJ.2017.35.2.1

Excel Download

Experimental Investigation of Laser Spot Welding of Ni and Au-Sn-Ni Alloy
Journal of Welding and Joining. 2017;35(2):1-5   Crossref logo
Link1 Link2 Link3

A comparative study of Pd/Sn/Au, Au/Ge/Au/Ni/Au, Au-Ge/Ni and Ni/Au-Ge/Ni ohmic contacts to n-GaAs
Microelectronic Engineering. 1998;40(1):35-42   Crossref logo
Link1 Link2

Autogenous fiber laser welding of 70/30 Cu-Ni alloy plates
Materials & Design. 2019;181:108075   Crossref logo
Link1 Link2

Experimental Investigation of Infrared Laser Drilling Process Applied with Different Repetition Rate on Ni-Au Coated BeCu
Journal of Welding and Joining. 2019;37(3):206-211   Crossref logo
Link1 Link2 Link3

ESCA study of the passive layer on Sn-Ni alloy
Vacuum. 1978;28(4):202   Crossref logo
Link1 Link2

Oxygen reduction activity of binary PtMn/C, ternary PtMnX/C (X = Fe, Co, Ni, Cu, Mo and, Sn) and quaternary PtMnCuX/C (X = Fe, Co, Ni, and Sn) and PtMnMoX/C (X = Fe, Co, Ni, Cu and Sn) alloy catalysts
Journal of Power Sources. 2013;236:311-320   Crossref logo
Link1 Link2

Experimental and theoretical investigation into visible-light-promoted selective hydrogenation of crotonaldehyde to crotonyl alcohol using Au–Co,Ni alloy nanoparticle supported layered double hydroxides
Journal of Materials Chemistry A. 2018;6(32):15839-15852   Crossref logo
Link1

Ultrasonic spot welding of aluminum alloys: A review
Journal of Manufacturing Processes. 2018;35:580-594   Crossref logo
Link1 Link2

Electrodeposition and electrochemical investigation of thin film Sn–Co–Ni alloy anode for lithium-ion batteries
Materials Science and Engineering: B. 2011;176(16):1329-1332   Crossref logo
Link1 Link2

Study on laser-tungsten inert gas hybrid welding of dissimilar Mg alloy and steel with Ni as interlayer
Materialwissenschaft und Werkstofftechnik. 2009;40(10):780-783   Crossref logo
Link1 Link2

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.