CrossRef Text and Data Mining
Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
The Effects of Microstructure on Cold Crack in High-Strength Weld Metals
Myung-Jin Lee, Nam-Hyun Kang
JWJ. 2014;32(1):22-27.   Published online 2014 February 27    DOI: https://doi.org/10.5781/JWJ.2014.32.1.22

Excel Download

Effects of Tempering on the Microstructure and Properties of a High-Strength Bainite Rail Steel with Good Toughness
Metals. 2018;8(7):484   Crossref logo
Link1

Investigation on Friction and Wear of Cold Rolled High Strength Steel against an AISI52100 Counterpart
Metals. 2017;7(3):90   Crossref logo
Link1

Size Effects of High Strength Steel Wires
Metals. 2019;9(2):240   Crossref logo
Link1

Characterization on the Microstructure Evolution and Toughness of TIG Weld Metal of 25Cr2Ni2MoV Steel after Post Weld Heat Treatment
Metals. 2018;8(3):160   Crossref logo
Link1

Fracture Assessment of the Weld–Base Metal Interface of High-Strength Steel Weld Joint
Strength of Materials. 2018;50(1):11-19   Crossref logo
Link1 Link2 Link3

Original test device for crack propagation in the weld nugget of advanced high strength steels
Engineering Fracture Mechanics. 2015;138:156-168   Crossref logo
Link1 Link2

Fatigue crack growth behavior in weld-repaired high-strength low-alloy steel
Engineering Fracture Mechanics. 2011;78(9):1862-1875   Crossref logo
Link1 Link2

Effects of pretest aging on creep crack growth properties of type 308 austenitic stainless steel weld metals
Engineering Failure Analysis. 2001;8(1):75-85   Crossref logo
Link1 Link2

Microstructure and Mechanical Properties of a High-Mn TWIP Steel Subjected to Cold Rolling and Annealing
Metals. 2017;7(12):571   Crossref logo
Link1

Application of cold drawn lamellar microstructure for developing ultra-high strength wires
Transactions of Nonferrous Metals Society of China. 2007;17(6):1129-1138   Crossref logo
Link1 Link2