Evaluation of Weldability based on Alignment Condition of Horns and Anvils used in Multilayered Battery Cell Welding Process in Ultrasonic Metal Welding
Seungmin Shin, Dongcheol Kim
J Weld Join. 2021;39(5):552-557.   Published online 2021 Sep 15     DOI: https://doi.org/10.5781/JWJ.2021.39.5.12
Citations to this article as recorded by Crossref logo
Review on Ultrasonic and Laser Welding Technologies of Multi-Layer Thin Foils for the Lithium-Ion Pouch Cell Manufacturing
Musung Kim, Heeseon Bang, Soongkeun Hyun, Sung Yi, Cheolhee Kim
Journal of Welding and Joining.2023; 41(6): 462.     CrossRef