Correlation Between HAZ Microstructure and Low Temperature Impact Toughness of Bainitic Steel Plates
Hun Lee, Sung Kyu Cho, Woo Hyuk Choi, Yang Gon Kim, Yong Jai Kwon, Jung Gu Lee, Sang Yong Shin, Dong Ki Choi
J Weld Join. 2021;39(3):269-277.   Published online 2021 Jun 28     DOI: https://doi.org/10.5781/JWJ.2021.39.3.5
Citations to this article as recorded by Crossref logo
Overcoming underfill defect with undermatching filler and establishing new acceptance criteria for underfill depth in laser beam welding of ultra-high strength steels
Yoona Lee, Sanghyeon Park, Jeongan Seon, Haksoo Han, Kwanghyeon Lee, Namhyun Kang
Welding in the World.2024; 68(2): 259.     CrossRef
Alleviation of Hydrogen Embrittlement to Delay Effective Hydrogen Diffusion Against MA Constituent Formation Due to Mo Solutes for 420 MPa Grade Offshore Steels
Jimin Nam, Junghoon Lee, Hanji Park, Cheolho Park, Changhoon Lee, Junho Chung, Seung-gun Lee, Namhyun Kang
Metals and Materials International.2023; 29(6): 1625.     CrossRef
Effects of Mo and Nb on Microstructure and Charpy Impact Properties of CGHAZ in HSLA Steels
Min Gu Kim, Sung Kyu Cho, Sang Yong Shin
Journal of Welding and Joining.2022; 40(1): 22.     CrossRef
A Study on the Microstructure and Mechanical Properties of the Coarse Grain Heat Affected Zone in EH40 Grade High Strength Structural Steels
Seonghoon Jeong, Seunglae Hong, JunSeok Seo, Ji-Hee Son, Hyung Goun Joo
Journal of Welding and Joining.2022; 40(5): 410.     CrossRef