A Comparison of Hot Cracking in GTAW and FCAW by Applying Alloy 625 Filler Materials of 9% Ni Steel
Ki Beom Na, Chang Ik Lee, Jung Hyun Park, Sang Myung Cho
J Weld Join. 2019;37(4):357-362.   Published online 2019 Jul 22     DOI: https://doi.org/10.5781/JWJ.2019.37.4.10
Citations to this article as recorded by Crossref logo
Quantifying Susceptibility to Solidification Cracking in Oscillated CM247LC Superalloy Welds via Varestraint Testing
Kyeong-Min Kim, Uijong Lee, Hyungsoo Lee, Seong-Moon Seo, Eun-Joon Chun
Metals and Materials International.2023; 29(3): 777.     CrossRef
A study on a representative heat source model for simulating laser welding for liquid hydrogen storage containers
Changmin Pyo, Jaewoong Kim, Younghyun Kim, Munsung Kim
Marine Structures.2022; 86: 103260.     CrossRef
Development and Evaluation of Stainless Steel-Base Flux-Cored Wires for 9% Nickel Steel
Tae-Uk Park, Young-Cheon Jeong, Hee-Dae Im, Chang-hyun Choi, Woong Kil
Journal of Welding and Joining.2022; 40(5): 367.     CrossRef
Bead Geometry Prediction Model for 9% Nickel Laser Weldment, Part 1: Global Regression Model vs. Modified Regression Model
Jisun Kim, Jaewoong Kim, Changmin Pyo, Kwangsan Chun
Processes.2021; 9(5): 793.     CrossRef
A Study on the Weldment Hardening Discrimination Procedure and Improvement of Flux Cored Arc Welding Process of ASTM A553-1 (9% Nickel Steel) Material Using Bead Geometry Distribution
Minho Park, Jisun Kim, Changmin Pyo, Jaewoong Kim, Kwangsan Chun
Metals.2021; 11(8): 1282.     CrossRef
A Study on Determining Weld Joint Hardening and a Quality Evaluation Algorithm for 9% Nickel Weld Joints Using the Dilution Ratio of the Base Material in Fiber Laser Welding
Minho Park, Jisun Kim, Changmin Pyo, Jaewoong Kim, Kwangsan Chun
Metals.2021; 11(8): 1308.     CrossRef
A Study on Welding Deformation in Fiber Laser Welding of 9% Nickel Steel through Finite Element Analysis Part I: Implementation of Welding Heat Source Model
Changmin Pyo, Jaewoong Kim, Du-Song Kim
Processes.2021; 9(12): 2188.     CrossRef
Experimental Study on Bead on Plate (BOP) Welding of 6 mm Thick 9% Nickel Steel by Fiber Laser Welding
Jaewoong Kim, Changmin Pyo, Yonghyun Kim, Sungwook Kang, Taegon Yeo, Kwangsan Chun, Du-Song Kim
Materials.2021; 14(24): 7699.     CrossRef
Laser Welding of ASTM A553-1 (9% Nickel Steel) (PART I: Penetration Shape by Bead on Plate)
Jaewoong Kim, Jisun Kim, Sungwook Kang, Kwangsan Chun
Metals.2020; 10(4): 484.     CrossRef
Laser Welding of ASTM A553-1 (9% Nickel Steel) (PART II: Comparison of Mechanical Properties with FCAW)
Jaewoong Kim, Jisun Kim
Metals.2020; 10(8): 999.     CrossRef
A Study on Cross-Shaped Structure of Invar Material Using Cold Wire Laser Fillet Welding (PART I: Feasibility Study for Weldability)
Du-Song Kim, Changmin Pyo, Jaewoong Kim, Jisun Kim, Hee-Keun Lee
Metals.2020; 10(10): 1385.     CrossRef