Effect of Composition on Strain-Induced Martensite Transformation and Tensile Stress-Strain Curve for Austenitic Stainless Steels
Ju Hyun Noh, Sang Gwon Lee, Hanji Park, Namhyun Kang
Journal of Welding and Joining. 2018;36(2):28-33. Published online 2018 Apr 30 DOI: https://doi.org/10.5781/JWJ.2018.36.2.5
|
Citations to this article as recorded by
Tensile and Microstructural Behaviors of Austenitic Stainless Steel GTA Welds for Cryogenic Application
Woosung Yang, Woong Kil, Byungrok Moon, Hyunbin Nam, Namhyun Kang
Journal of Welding and Joining.2020; 38(4): 400. CrossRef
|