Latest Technology of Non Destructive Inspection for Welded Structure
Youngsik Kim, Sangcheol Kil
J Weld Join. 2017;35(2):63-70.   Published online 2017 Apr 28     DOI: https://doi.org/10.5781/JWJ.2017.35.2.10
Citations to this article as recorded by Crossref logo
Feature Analysis Based on Acoustic Emission Signal Processing for Tubular Steel Tower Condition Monitoring
Hyeon-Tak Yu, Tae-Hong Min, Hyeong-Jin Kim, Seoggeun Kang, Dong-Young Kang, Hyun-Sik Kim, Byeong-Keun Choi
Transactions of the Korean Society for Noise and V.2021; 31(2): 195.     CrossRef
Extracting Weld Bead Shapes from Radiographic Testing Images with U-Net
Gang-soo Jin, Sang-jin Oh, Yeon-seung Lee, Sung-chul Shin
Applied Sciences.2021; 11(24): 12051.     CrossRef