A Study of Characteristics on the Dissimilar Metals (STS 316L - Carbon Steel: ASTM A516-70) Welds made with GTAW
Se Cheol Kim, Tae Woo Shin, In Joon Moon, Bok Su Jang, Jin Hyun Koh
Journal of Welding and Joining. 2015;33(4):37-43.   Published online 2015 Aug 31     DOI: https://doi.org/10.5781/JWJ.2015.33.4.37
Citations to this article as recorded by Crossref logo
A Study of Characteristics on the Dissimilar Metals (ASTM Type 316L - Carbon Steel : ASTM A516-70) Welds Made with FCA Multiple Layer Welding
Se Cheol Kim, Jun Hyeok Hyun, Tae Woo Shin, Jin Hyun Koh
Journal of Welding and Joining.2016; 34(3): 69.     CrossRef