Weldability Increase of Aluminum by Variable Polarity Arc
Jungho Cho
J Weld Join. 2014;32(1):108-111. Published online 2014 Feb 27 DOI: https://doi.org/10.5781/JWJ.2014.32.1.108
|
Citations to this article as recorded by
Optimization of Welding Process Parameter for Gap Response in Aluminum GMAW Using Taguchi Method
Hyojun Choi, Taehoon Kang, Jiyoung Yu, Young-Min Kim, Seung Hwan Lee, Dong-Yoon Kim
Journal of Welding and Joining.2023; 41(1): 28. CrossRef Effect of weld geometry on fatigue performance of 6061-T6 aluminum GMAW: part 3. T-fillet joint
Sang Woo Han, Geonho Lee, Hansol Kim, Min Soo Kim, Young Rae Jo, Jungho Cho
Journal of Mechanical Science and Technology.2022; 36(10): 5215. CrossRef Effect of weld geometry on fatigue performance of 6061-T6 aluminum GMAW: part 1. Butt joint
Sang-Woo Han, Geonho Lee, Hansol Kim, Min-Soo Kim, Young-Rae Jo, Jungho Cho
Journal of Mechanical Science and Technology.2022; 36(10): 5201. CrossRef Effect of weld geometry on fatigue performance of 6061-T6 aluminum GMAW: part 2. Lap joint
Sang-Woo Han, Geonho Lee, Hansol Kim, Min-Soo Kim, Young-Rae Jo, Jungho Cho
Journal of Mechanical Science and Technology.2022; 36(10): 5209. CrossRef Effect of Aluminum Arc Butt Joint Weld Geometry on Fatigue Strength
Jungho Cho, Sungjin Baek, Seungchul Shin, Gunho Lee, Mun-Gu Kang, Young-Rae Jo
Journal of Welding and Joining.2021; 39(1): 103. CrossRef Cathode Spot Phenomena Observation by High Speed Camera
in Variable Polarity Aluminum Arc Welding
Jungho Cho, Huncheol Jung, Kyungbae Park, Junkyung Lee
Journal of Welding and Joining.2018; 36(1): 103. CrossRef Numerical analysis of variable polarity arc weld pool
Hunchul Jeong, Kyunbae Park, Jungho Cho
Journal of Mechanical Science and Technology.2016; 30(9): 4307. CrossRef
|