In this issue:


Special Issue
537 Weld Quality Evaluation Method for the Resistance Spot Welds using X-ray Transmission Inspection   
Jong-Dae Lee, So-Jeong Lee, Jung-Hwan Bang, Gil-Sang Yoon, Mok-Soon Kim, Jun-Ki Kim
Journal of Welding and Joining:537-543.  Publication Date (Web): December 31, 2014
PDF Links
 
544 A Study on Development of STACO Model to Predict Bead Height in Tandem GMA Welding Process   
Jongpyo Lee, IllSoo Kim, Minho Park, Cheolkyun Park, Bongyong Kang, Jiyeon Shim
Journal of Welding and Joining:544-549.  Publication Date (Web): December 31, 2014   Cited by 1
PDF Links
 
550 Prediction of Cr Content in the Martensitic-hardfaced Weldment Utilizing Dilution Rate Analytically Estimated   
Bong-Hun Kim, Chun-Hwan Kim
Journal of Welding and Joining:550-557.  Publication Date (Web): December 31, 2014
PDF Links
 
Research Paper
558 Influence of Surface Roughness of Tools on the Friction Stir Welding Process   
Michael Hartmann, Stefan Böhm, Sven Schüddekopf
Journal of Welding and Joining:558-564.  Publication Date (Web): December 31, 2014   Cited by 2
PDF Links
 
565 Effects of C on the Strength and Toughness of FCAW Weld Metal of YS 460 MPa Steels for Ship and Offshore Structures   
Sang-Hoon Jeong, Jeong-Ho Eom, Han-Geul Choi, Byung-Ho Jeong, Sung-Hwa Hur, Chang-Yong Kang
Journal of Welding and Joining:565-570.  Publication Date (Web): December 31, 2014   Cited by 1
PDF Links
 
571 Evaluation of Gas Metal Arc Welding Characteristics according to Contact Tip Materials   
Dong Yoon Kim, In Sung Hwang, Dong Cheol Kim, Moon Jin Kang
Journal of Welding and Joining:571-576.  Publication Date (Web): December 31, 2014
PDF Links
 
577 Cracking Susceptibility of Laser Cladding Process with Co-Based Metal Matrix Composite Powders   
Changmin Lee, Hyungkwon Park, Changhee Lee
Journal of Welding and Joining:577-582.  Publication Date (Web): December 31, 2014   Cited by 3
PDF Links
 
583 Effects of GTAW Pulse Condition on Penetration, Discoloration and Bending Property for Titanium Tube   
Seonghwan Min, Sungyong An, Jitae Park, Youngdo Park, Namhyun Kang
Journal of Welding and Joining:583-591.  Publication Date (Web): December 31, 2014   Cited by 2
PDF Links
 
592 A Study on the Characteristic of Weld Joint and Tensile Fracture of SUS304 and Cu High-Speed Dissimilar Lap Welds by Single Mode Fiber Laser   
Su-Jin Lee, Jong-Do Kim, Seiji Katayama
Journal of Welding and Joining:592-599.  Publication Date (Web): December 31, 2014   Cited by 1
PDF Links
 
600 A Study on Correlationship between the Induced Plasma and Emission Signals for In-process Monitoring in Stainless Steel Welding of Fiber Laser (Ⅰ)
- Properties Changes of the Measured Signals in a Thin Plate Welding -
  
Chang-Je Lee, Jong-Do Kim
Journal of Welding and Joining:600-605.  Publication Date (Web): December 31, 2014
PDF Links
 
606 A Study on Correlationship between the Induced Plasma and Emission Signals for In-process Monitoring in Stainless Steel Welding of Fiber Laser (Ⅱ)
- Properties Changes of the Measured Signals in a Thick Plate Welding -
  
Chang-Je Lee, Jong-Do Kim
Journal of Welding and Joining:606-610.  Publication Date (Web): December 31, 2014
PDF Links
 
611 Degradation Behavior of Eutectic and Pb-free Solder Plated Ribbon in Crystalline Silicon Photovoltaic Module   
Ju-Hee Kim, A Yong Kim, Nochang Park, Jeong Won Ha, Sang Guon Lee, Won Sik Hong
Journal of Welding and Joining:611-617.  Publication Date (Web): December 31, 2014
PDF Links
 
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.