Advanced Search  
  Previous issue

Table of Contents | December, 2013  Vol. 31  No.6 Previous Issue | Next Issue | Archive
In this issue:




Special Issue
1 Butt-fusing Procedures and Qualifications of High Density Polyethylene Pipe for Nuclear Power Plant Application   
Young-Jin Oh, Heung-Bae Park, Ho-Sang Shin
Journal of Welding and Joining:1-7.  Publication Date (Web): January 21, 2014
PDF Links
 
8 The Effects of δ-ferrite on Weldment of 9-12% Cr Steels   
Sung-Yong Ahn, Namhyun Kang
Journal of Welding and Joining:8-16.  Publication Date (Web): January 21, 2014   Cited by 2
PDF Links
 
Review Paper
17 Recent Study in Variation of Welding Materials for Overlay Welding   
Ho-Cheon Yoo
Journal of Welding and Joining:17-26.  Publication Date (Web): January 21, 2014   Cited by 2
PDF Links
 
Technical report
27 Electrode Life Test of Resistance Spot Welding on Mg Alloy Using Dome Type Electrode   
Dong-Soon Choi, In-Sung Hwan, Dong-Cheol Kim, Moon-Jin Kang
Journal of Welding and Joining:27-31.  Publication Date (Web): January 21, 2014   Cited by 2
PDF Links
 
Research Paper
32 A Study on Prediction of Fatigue Life using MFC Sensors   
Ji-Hoon Lee, Dong-Jin Oh, Myung-Hyun Kim
Journal of Welding and Joining:32-36.  Publication Date (Web): January 21, 2014
PDF Links
 
37 A Study on Analyzing Thermal Strain of Weldment during Cooling used at Low MS Point Weld Consumables   
Yunsok Ha, Seongkil Nam, Sejin Park, Changgil Kwon
Journal of Welding and Joining:37-43.  Publication Date (Web): January 21, 2014
PDF Links
 
44 Microstructure Evolution and Its Effect on Strength during Thermo-mechanical Cycling in the Weld Coarse-grained Heat-affected Zone of Ti-Nb Added HSLA Steel   
Joonoh Moon, Changhee Lee
Journal of Welding and Joining:44-49.  Publication Date (Web): January 21, 2014   Cited by 4
PDF Links
 
50 A Study on Microstructures and Cryogenic Mechanical Properties of Electron Beam Welds between Cast and Forged Inconel 718 Superalloys for Liquid Rocket Combustion Head   
Hyun-Uk Hong, Sang-Hyun Bae, Soon-Il Kwon, Je-Hyun Lee, Jeong-Hyeon Do, Baig-Gyu Choi, In-Soo Kim, Chang-Yong Jo
Journal of Welding and Joining:50-57.  Publication Date (Web): January 21, 2014
PDF Links
 
58 Laser Welding Characteristics of Aluminum and Copper Sheets for Lithium-ion Batteries   
Minjung Kang, Taesoon Park, Cheolhee Kim, Jeonghan Kim
Journal of Welding and Joining:58-64.  Publication Date (Web): January 21, 2014   Cited by 1
PDF Links
 
65 The Effect of the Composition of Metallizing Paste on the Bonding Strength in the Joining of Al2O3 to Cu   
Jong-Hyuk Yoon, Hyun Gyoon Park
Journal of Welding and Joining:65-70.  Publication Date (Web): January 21, 2014
PDF Links
 
71 Porosity Reduction in Laser Welding of Nitrided Carbon Steel   
Young-Nam Ahn, Cheolhee Kim, Wonbeom Lee, Jeonhan Kim
Journal of Welding and Joining:71-76.  Publication Date (Web): January 21, 2014   Cited by 1
PDF Links
 
77 Fracture Mode Analysis with ISB Bonding Process Parameter for 3D Packaging   
Young-Kang Lee, Jae-Hak Lee, Jun-Yeob Song, Hyoung-Joon Kim
Journal of Welding and Joining:77-83.  Publication Date (Web): January 21, 2014
PDF Links
 
84 Effects of High Current and Welding Wire Diameter on the Magnesium Vaporization and Mechanical Properties of Al5083 Arc Welds   
Heimi Kwon, Chul-ho Park, In-Pyo Hong, Namhyun Kang
Journal of Welding and Joining:84-89.  Publication Date (Web): January 21, 2014
PDF Links
 
90 Development of Welding Quality Monitoring Method for TIG Cladding   
Sang Myung Cho, Min Su Son, Jung Hyun, Park
Journal of Welding and Joining:90-95.  Publication Date (Web): January 21, 2014   Cited by 2
PDF Links
 
96 Effect of Hot-stamping on Microstructures and Tensile Properties of Al-Si Coated Boron Steel Welds with Laser Source   
Myeong-Hwan Oh, Jong-Pan Kong, Min-Suck Kwon, Chung-Yun Kang
Journal of Welding and Joining:96-106.  Publication Date (Web): January 21, 2014   Cited by 5
PDF Links
 
107 A Study on the Welding Distortion Analysis According to Rib Height in Fillet Welding   
Yong-Rae Kim, Gyu-Yeong Song, Chao Wang, Jae-Woong Kim
Journal of Welding and Joining:107-111.  Publication Date (Web): January 21, 2014
PDF Links
 
112 Hydrogen Embrittlement Resistance and Diffusible Hydrogen Desorption Behavior of Multipass FCA Weld Metals   
Jaeseok Yoo, Guo Xian, Myungjin Lee, Yongdeok Kim, Namhyun Kang
Journal of Welding and Joining:112-118.  Publication Date (Web): January 21, 2014   Cited by 3
PDF Links
 
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.