5 Cracking in Welds and Its Prevention(VII)
박화순
Journal of Welding and Joining:5-7.  Publication Date (Web): February 25, 2003
PDF Links
 
8 Effect of Microstructure on Cold Crackin in Weld Metal
김희진, 강봉용
Journal of Welding and Joining:8-13.  Publication Date (Web): February 25, 2003
PDF Links
 
14 Trend in Digitalization of Welding Power Source and Application of Information Technology
강문진, 강봉용, 김정한
Journal of Welding and Joining:14-20.  Publication Date (Web): February 25, 2003
PDF Links
 
21 Application of Waveform Control Technology in GMA Welding
김희진, 유회수, 강봉용
Journal of Welding and Joining:21-26.  Publication Date (Web): February 25, 2003
PDF Links
 
27 Waveform Control and Welding Characteristies in Pulse Arc Welding Process
조상명
Journal of Welding and Joining:27-34.  Publication Date (Web): February 25, 2003
PDF Links
 
35 Snubber Design and Device Parallel Operation for High Frequency Welding Machine
김태진
Journal of Welding and Joining:35-41.  Publication Date (Web): February 25, 2003
PDF Links
 
42 A Study on the Development of Insulated Electrode Tip for Sprot Welding to Reduce Indentation
서승일, 장상길
Journal of Welding and Joining:42-47.  Publication Date (Web): February 25, 2003
PDF Links
 
48 Effect of Short Circuit Time Ratio and Current Control Pattern on Spatter Generation in CO2 Welding
조상명
Journal of Welding and Joining:48-53.  Publication Date (Web): February 25, 2003
PDF Links
 
54 Estimation of Plate Deformation in Thermal Processing using the Eigenstrain Concept
손광제, 양영수, 장상균
Journal of Welding and Joining:54-59.  Publication Date (Web): February 25, 2003
PDF Links
 
60 A Study on Seam Tracking and Weld Defects Detecting for Automated pipe Welding by Using Double Vision Sensors
송형진, 이승기, 강윤희, 나석주
Journal of Welding and Joining:60-65.  Publication Date (Web): February 25, 2003
PDF Links
 
66 A Study on Non-linear Behavior in Welded Structures by Mechanical Stress Release Method
김정현, 장경복, 윤훈성, 강성수, 조상명
Journal of Welding and Joining:66-71.  Publication Date (Web): February 25, 2003
PDF Links
 
72 Fatigue Crack Propagation Life of Partially Penetrated Butt Welds in High Strength Steel
한승호, 신병천, 이웅, 최전호
Journal of Welding and Joining:72-79.  Publication Date (Web): February 25, 2003
PDF Links
 
80 Predictive System Evaluation of Residul Stresses of Plate Butt Welding Using Neural Network
차용훈, 성백섭, 이연신
Journal of Welding and Joining:80-86.  Publication Date (Web): February 25, 2003
PDF Links
 
87 Strength Characteristics of Reduced Activation Ferritic Steel for Fusion Blanket by TIG Welding
윤하기, 이상필, 김동현, A Kohyama
Journal of Welding and Joining:87-92.  Publication Date (Web): February 25, 2003
PDF Links
 
93 A Fundamental Study on Forecast of the Thin Plate Welding Deformation by Numerical Simulation
김종명, 박창수, 김영표, 방한서
Journal of Welding and Joining:93-98.  Publication Date (Web): February 25, 2003
PDF Links
 
99 A Study on Advanced Small Punch Test for Evaluation of Material Degradation in Weldment Microstructures
이동환, 이송인, 박종진, 유효선
Journal of Welding and Joining:99-106.  Publication Date (Web): February 25, 2003
PDF Links
 
107 A Study for Joining of Silicon Nitride with Crystallized Glass Soder of SiO2-Al2O3-MgO System
안병국
Journal of Welding and Joining:107-113.  Publication Date (Web): February 25, 2003
PDF Links
 
114 (주)포스코 기술연구소 용접연구팀
편집부
Journal of Welding and Joining:114-115.  Publication Date (Web): February 25, 2003
PDF Links
 
116 학회소식
편집부
Journal of Welding and Joining:116-123.  Publication Date (Web): February 25, 2003
PDF Links
 
124 회원사 동정
편집부
Journal of Welding and Joining:124-130.  Publication Date (Web): February 25, 2003
PDF Links
 
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.