In this issue:

1 Welding on Ship Building and Offshore Structure
김대순
Journal of Welding and Joining:1-6.  Publication Date (Web): October 25, 2002
PDF Links
 
7 Application of Welding Technoloby to Automotive Industry
오연근, 박현성
Journal of Welding and Joining:7-11.  Publication Date (Web): October 25, 2002
PDF Links
 
12 Advanced Welding Processes for Line Pipes and Their Prospects
김충명
Journal of Welding and Joining:12-18.  Publication Date (Web): October 25, 2002
PDF Links
 
19 State of the Art in the Manufacture of Heavy Forging Reactor Vessel
지병하, 김정태, 박화순
Journal of Welding and Joining:19-28.  Publication Date (Web): October 25, 2002
PDF Links
 
29 Investigation of Welding joint-Design and Technique for 9%Ni Steel of LNG Storage Tank
김형식, 김우식
Journal of Welding and Joining:29-35.  Publication Date (Web): October 25, 2002
PDF Links
 
36 Application of Welding and joining Technology for Aircrft and Aerospace Industry
김대엄
Journal of Welding and Joining:36-41.  Publication Date (Web): October 25, 2002
PDF Links
 
42 Trends and Prospects of Domestic Joining Technology in Electric. Electronic Field
신영의, 고영욱
Journal of Welding and Joining:42-51.  Publication Date (Web): October 25, 2002
PDF Links
 
52 Cracking in Welds and Its Prevention(v)
박화순
Journal of Welding and Joining:52-54.  Publication Date (Web): October 25, 2002
PDF Links
 
55 Consideration on Preheating Temperature Criteria for HY-Steels
김희진, 강봉용
Journal of Welding and Joining:55-62.  Publication Date (Web): October 25, 2002
PDF Links
 
63 Effects of Nitrogen and Precipitates on the Mechanical Properties of 26Cr 2Mo Superferritic Stainless Steel Welds
황의순, 이하미, 김성욱, 이창희, 안상곤, 이용득, 이용득
Journal of Welding and Joining:63-71.  Publication Date (Web): October 25, 2002
PDF Links
 
72 Aging Characteristic of Shear Strength in Micro Solder Bump
김경섭, 유정희, 선용빈
Journal of Welding and Joining:72-77.  Publication Date (Web): October 25, 2002
PDF Links
 
78 Austenite Grain Growth Prediction Modeling of C-Mn-Mo-Ni Steel HAZ Considering Precipitates
서영대, 엄상호, 이창희, 김주학, 홍준화
Journal of Welding and Joining:78-86.  Publication Date (Web): October 25, 2002
PDF Links
 
87 The Effects of Welding Conditions on the joint Properties of the Friction Stir Weded AZ31B-H24 Mg Alloys
이원배, 방극생, 연윤모, 정승부
Journal of Welding and Joining:87-92.  Publication Date (Web): October 25, 2002
PDF Links
 
93 Effect of Bonding Misfit on Single Crystallization of Transient Liquid Phase Bonded Joints of Ni Base Single Crystal Superalloy
김대업
Journal of Welding and Joining:93-98.  Publication Date (Web): October 25, 2002
PDF Links
 
99 Evaluation of Environmental Fatigue Strength in Adhesive Bonding of Different Materials
임재규, 이중삼, 윤호철, 유성철
Journal of Welding and Joining:99-105.  Publication Date (Web): October 25, 2002
PDF Links
 
106 The Wetting Property of Indium Soder
김대곤, 이창배, 정승부
Journal of Welding and Joining:106-112.  Publication Date (Web): October 25, 2002
PDF Links
 
113 Development of a Program for Prediction and Visualization of Welding Deformations
서승일, 노재규, 이정수
Journal of Welding and Joining:113-119.  Publication Date (Web): October 25, 2002
PDF Links
 
120 Optimization of the Plasma Spray Coating Parameters of Ni-5%AI Alloy Powder
이형근
Journal of Welding and Joining:120-126.  Publication Date (Web): October 25, 2002
PDF Links
 
127 Metal Transfer Characteristics of Aluminium under Pulsed Current Metal Inert Gas Welding
최재호, 최병도, 김용석
Journal of Welding and Joining:127-133.  Publication Date (Web): October 25, 2002
PDF Links
 
134 현대모비스(주) 기술연구소 재료시험 연구실
편집부
Journal of Welding and Joining:134-135.  Publication Date (Web): October 25, 2002
PDF Links
 
136 대한용접학회/2002년도 정기총회 및 추계학술대회 개최 안내
편집부
Journal of Welding and Joining:136-143.  Publication Date (Web): October 25, 2002
PDF Links
 
144 회원사동정
편집부
Journal of Welding and Joining:144-148.  Publication Date (Web): October 25, 2002
PDF Links
 
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.