Stress Concentration on Weldments
김응준
J Weld Join. 1989;7(3):1-6.   Published online September 25, 1989
PDFPDF    
The manufacturing of clad steel and its utilization
최영국
J Weld Join. 1989;7(3):7-18.   Published online September 25, 1989
PDFPDF    
The Study on Dynamic Fracture Toughness of Friction Welded M.E.F Dual Phase Steel
오세욱, 유재환, 이경봉
J Weld Join. 1989;7(3):19-27.   Published online September 25, 1989
PDFPDF    
A Study on Fracture Strength Evaluation of Steel Welded Joint by Small Punch Test I
유대영, 정세희, 임재규, 정희돈, 玉川欣治, 高橋秀明
J Weld Join. 1989;7(3):28-35.   Published online September 25, 1989
PDFPDF    
Effect of Sn and P on the Shear Strength of Copper to Stainless Steel Brazed Joint
정재필, 이보영, 이우천, 강춘식
J Weld Join. 1989;7(3):36-43.   Published online September 25, 1989
PDFPDF    
Effects of Microstructure and Welding Heat Input on the Toughness of Weldable High Strength Steel Weldments
장웅성, 방국수, 장래웅, 엄기원
J Weld Join. 1989;7(3):44-54.   Published online September 25, 1989
PDFPDF    
A Study on the Formation and Mechanical Properties of the Spray Deposits by Thermal Spray
최기영, 박동환, 김명호
J Weld Join. 1989;7(3):55-62.   Published online September 25, 1989
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI