42 The Effects of Nitrogen Content and Cold rolling reduction on the Mechanical Properties of New 420-series Stainless Steel Strip having a Mesh As-Welded Structure by the Electroslag Cladding   
Jae-Young Jung
Journal of Welding and Joining:42-50.  Publication Date (Web): November 13, 2017   Cited by 2
PDF Links
 
42 The Effects of Nitrogen Content and Cold Rolling Reduction on the Mechanical Properties of New 420-series Stainless Steel Strip having a Mesh As-Welded Structure by the Electroslag Cladding   
Jae-Young Jung
Journal of Welding and Joining:42-50.  Publication Date (Web): December 31, 2017
                  PDF Links
 
32 Variations of Chemical Composition and Effects of Welding Parameters on the Overlay Welding Behaviors and Fluxes in Electroslag Cladding by using a New 420-series Stainless Steel Strip   
Jae-Young Jung, Eung Ryul Baek
Journal of Welding and Joining:32-41.  Publication Date (Web): December 5, 2017
                  PDF Links
 
77 Effects of Welding Parameters on the Overlay Welding Behaviors in Electroslag Cladding by using AISI 430 Stainless Steel Strip - Experimental Study   
Jae-Young Jung, Tae-Kwon Ha
Journal of Welding and Joining:77-86.  Publication Date (Web): October 27, 2017   Cited by 3
                  PDF Links
 
48 The Changes of Chemical Composition and Microstructure in Electroslag Cladding Overlays by using AISI 430 Stainless Steel Strip   
Jae-Young Jung, Tae-Kwon Ha
Journal of Welding and Joining:48-56.  Publication Date (Web): September 13, 2017   Cited by 3
                  PDF Links
 
1 |
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.