Advanced Search  
 JWJ Search

593 A Study on the Prediction of Real-Time Bead Width Using a DNN Algorithm in GTA Welding   
Won-Bin Oh, Ill-Soo Kim, Tae-Jong Yun, Bo-Ram Lee, Chung-Woo Lee, Ki-Young Park, Byeong-Ju Jin, Yu-Cheol Lee
Journal of Welding and Joining:593-601.  Publication Date (Web): December 14, 2020
                  PDF Links
 
90 Development of Welding Quality Monitoring Method for TIG Cladding   
Sang Myung Cho, Min Su Son, Jung Hyun, Park
Journal of Welding and Joining:90-95.  Publication Date (Web): January 21, 2014   Cited by 2
PDF Links
 
1 |
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI