Search

  • HOME
  • Search
2032280
Solidification Crack Free Welding Strategy via Ultra High Precision Laser Scanning at a Single Grain of Directionally Solidified and Single Crystal Superalloys
Seong-Jin Lee, Kyeong-Min Kim, Heeshin Kang, Seong-Moon Seo, Wonah Park, Eun-Joon Chun
J Weld Join. 2023;41(4):254-264.   Published online August 31, 2023
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Transient Liquid Phase Bonding of Gamma Prime Precipitation Strengthened Ni Based Superalloy
Jeong Kil Kim, Hae Ji Park, Deog Nam Shim
J Weld Join. 2017;35(3):52-61.   Published online June 30, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Microstructure and Creep Fracture Characteristics of Dissimilar SMA Welds between Inconel 740H Ni-Based Superalloy and TP316H Austenitic Stainless Steel
Kyeong-Yong Shin, Ji-Won Lee, Jung-Min Han, Kyong-Woon Lee, Byeong-Ook Kong, Hyun-Uk Hong
J Weld Join. 2016;34(5):33-40.   Published online October 30, 2016
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Effects of Post Weld Heat Treatment on Microstructures of Alloy 617 and 263 Welds for Turbines of HSC Power Plants
Jeong Kil Kim, Deog Nam Shim, Hae Ji Park
J Weld Join. 2016;34(3):52-60.   Published online June 30, 2016
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031710
Fatigue Life of the Repair TIG Welded Hastelloy X Superalloy
Restu SIHOTANG, Sang-Kyu CHOI, Sung-Sang PARK, Eung-Ryul BAEK
J Weld Join. 2015;33(5):26-30.   Published online October 30, 2015
PDFPDF    
Effect of Bonding Condition on the Tensile Properties of Diffusion Bonded Haynes230
Gil-Mo Kang, Ae-Jeong Jeon, Hong-Kyu Kim, Sung-Suk Hong, Chung-Yun Kang
J Weld Join. 2013;31(3):76-83.   Published online June 30, 2013
PDFPDF    
The Bonding Strength Characteristic of the Filler Metal Powder on the TLP Bonded Region of Superalloy GTD-111DS
In-Seok Oh, Gil-Moo Kim, Byeong-Shik Moon
J Weld Join. 2007;25(5):45-50.   Published online December 3, 2007
PDFPDF    
Dissolution Phenomenon of the Base Metal during TLP Bonding Using the Modified Base Metal Powder and Ni Base Filler Metal Powder
Woo-young Song, Chang-ho Ye, Chung-yun Kang
J Weld Join. 2007;25(3):64-71.   Published online July 19, 2007
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI