67 Fuzzy Logic Optimization for Low Sulphur and Phosphorus in Submerged Arc Weldments   
Brijpal Singh
Journal of Welding and Joining:67-72.  Publication Date (Web): December 5, 2017
                  PDF Links
 
7 Development of Structural Steel and Trend of Welding Technology   
Sung Jin Kim, Hong Chul Jeong
Journal of Welding and Joining:7-20.  Publication Date (Web): February 29, 2016   Cited by 1
                  PDF Links
 
431 Evaluation of HIC/SSCC Resistance for API-X70 Pipe Manufactured by JCO Bending Process and SA Welding   
Hoi-Soo Ryoo, Hee Jin Kim, Dong-Eon Lee
Journal of Welding and Joining:431-436.  Publication Date (Web): October 30, 2014
PDF Links
 
93 Effect of Heat Input of Outside Weld on Low Temperature Toughness of Inside Weld for Multiple Electrode SA Welded API 5L X70 with Sour Gas Resistance   
Hyun-Jun An, Hee-Keun Lee, Young-Gyu Park, Seong-Su Eun, Chung-Yun Kang
Journal of Welding and Joining:93-101.  Publication Date (Web): February 27, 2014   Cited by 1
PDF Links
 
15 Evaluation on Mechanical Properties with Welding Processes for Off Shore Wind Tower Application   
Changwook Ji, Chul Young Choi, Dae-Geun Nam, Hyoung Chan Kim, Jae Ho Jang, Ki Hyuk Kim, Yeong-Do Park
Journal of Welding and Joining:15-21.  Publication Date (Web): February 27, 2014
PDF Links
 
6 Evaluation and Comparison of Weldabilities with Various Welding Processes on TMCP Steels   
Chul Young Choi, Chang Wook Ji, Hyoung Chan Kim, Dae-Geun Nam, Joungdon Kim, Soon Kook Kim, Yeong-Do Park
Journal of Welding and Joining:6-14.  Publication Date (Web): February 27, 2014
PDF Links
 
47 Evaluation of Corrosion Resistance and Weldability for the Butt Welding Zone of Hot Rolled Clad Steel Plates   
Jae-Won Park, Chul-ku Lee
Journal of Welding and Joining:47-53.  Publication Date (Web): November 5, 2013
PDF Links
 
49 The Sensitization and Intergranular Corrosion Behavior of AISI 316L Clad Steel with Butt Welding   
Chul-ku Lee, Jae-Won Park
Journal of Welding and Joining:49-56.  Publication Date (Web): June 5, 2013   Cited by 2
PDF Links
 
11 Recent Study of Overlay Welding on Welding methods   
Ho-Cheon Yoo
Journal of Welding and Joining:11-20.  Publication Date (Web): June 4, 2013   Cited by 1
PDF Links=
 
     Comparison of GMAW and SAW for NGW of 50 mm Q&T Steel Plate   
Druce Patrick Dunne, Willy Pang
  Publication Date (Web): January 22, 2018
[Epub ahead of print]
PDF Links
 
     Correlation of Flux Ingredients with HAZ Width in Submerged Arc Welding   
Brijpal Singh
  Publication Date (Web): February 14, 2018
[Epub ahead of print]
PDF Links
 
1 |
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.