591 Formation of Intermetallic Compounds at the Interface of the Friction Stir Weld and Diffusion Bond of Mg-AZ31/Al-5083 Joint   
Mohammad Ammar Mofid, Ehsan Loryaei, Mostafa Hajian Heidary
Journal of Welding and Joining:591-598.  Publication Date (Web): December 5, 2019
                  PDF Links
 
196 Resistance Spot Welding Characteristics of Mg Alloy Applying Current Waveform Control   
Dong-Soon Choi, In-Sung Hwang, Dong-Cheol Kim, Jae-Wook Ryu, Moon-Jin Kang
Journal of Welding and Joining:196-201.  Publication Date (Web): May 14, 2014
PDF Links
 
27 Electrode Life Test of Resistance Spot Welding on Mg Alloy Using Dome Type Electrode   
Dong-Soon Choi, In-Sung Hwan, Dong-Cheol Kim, Moon-Jin Kang
Journal of Welding and Joining:27-31.  Publication Date (Web): January 21, 2014   Cited by 2
PDF Links
 
7 Effects of the Types of Coating on the Laser Brazing Characteristics of Dissimilar Joints between Mg Alloy and Steel Sheet   
Mok-Young Lee, Sook-Whan Kim, ALI M. NASIRI, NORMAN Y. ZHOU
Journal of Welding and Joining:7-12.  Publication Date (Web): August 31, 2013
PDF Links
 
49 Resistance Spot Welding Characteristics of Mg Alloy Using Process Tape   
Dong-Soon Choi, Dong-Cheol Kim, Moon-Jin Kang
Journal of Welding and Joining:49-53.  Publication Date (Web): June 30, 2013   Cited by 2
PDF Links
 
80 Prevention of Back Side Humping in Laser Welding of Al 5J32 Alloy by Using Laser Power Modulation
Do-Chang Ahn, Cheolhee Kim, Jaedo Kim
Journal of Welding and Joining:80-84.  Publication Date (Web): September 12, 2011
PDF Links
 
80 Effects of Tool Speed on Joining Characteristics during Friction Stir Spot Welding of Mg-alloy(AZ31B) Sheet
Hyung-Seop Shin, Yoon-Chul Jung, Kwang Choi
Journal of Welding and Joining:80-87.  Publication Date (Web): May 7, 2011
PDF Links
 
102 A Study on Servo DC Resistance Spot Welding of Mg Alloy Sheet(1)
SunNyeo Jung, HeeSeok Chang, Mok-Young Lee
Journal of Welding and Joining:102-107.  Publication Date (Web): March 12, 2009
PDF Links
 
54 Laser Welding of AZ31B-H24 Mg Alloy with AZ61 Filler Wire
Chung-Sun Ryu, Kook-Soo Bang, Mok-Young Lee, Woong-Sung Chang
Journal of Welding and Joining:54-58.  Publication Date (Web): January 13, 2009
PDF Links
 
1 |
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.