Advanced Search  
 JWJ Search

485 A Study on Optimization of Fillet in Laser Welding Process for 9% Ni Steel Using Gradient-Based Optimization Algorithm   
Tae-Jong Yun, Won-Bin Oh, Bo-Ram Lee, Chung-Woo Lee, Hyun-Ho Na, Ju-Seok Choi, Ill-Soo Kim
Journal of Welding and Joining:485-492.  Publication Date (Web): September 24, 2020
                  PDF Links
 
469 A Study on Process Robustness of Lap Joint Fillet Welding in GTAW Using C Type Filler   
Sang-Yeol Kim, Gi-Jeong Seo, Woo-Hyeon Ju, Sang-Myung Cho
Journal of Welding and Joining:469-476.  Publication Date (Web): September 30, 2019
                  PDF Links
 
52 Development of Quality Inspection System for Fillet Welding Based on Laser Vision Sensor   
Ui-Tae Jeong, Hyeong-Jun Lee, In-Soo Lee
Journal of Welding and Joining:52-59.  Publication Date (Web): December 5, 2018
                  PDF Links
 
48 Porosity Reduction during Gas Tungsten Arc-Gas Metal Arc Hybrid Welding of Zinc Coated Steel Sheets (II) - Hybrid Welding Results   
Young-Nam Ahn, Cheolhee Kim
Journal of Welding and Joining:48-54.  Publication Date (Web): August 23, 2016   Cited by 3
                  PDF Links
 
40 Porosity Reduction during Gas Tungsten Arc-Gas Metal Arc Hybrid Welding of Zinc Coated Steel Sheets (I) - Effect of Preceding Gas Tungsten Arc   
Minjung Kang, Young-Nam Ahn, Cheolhee Kim
Journal of Welding and Joining:40-47.  Publication Date (Web): August 23, 2016   Cited by 1
                  PDF Links
 
163 A Study of the Thickness Effect using Structural Stress Approach for Fillet Welded Joints   
Wen-Jie Xin, Dong-Jin Oh, Myung-Hyun Kim
Journal of Welding and Joining:163-168.  Publication Date (Web): May 14, 2014   Cited by 3
PDF Links
 
79 A Study on Design of Fillet Weld Size for Stiffener in the Hull Bottom of Crude Oil Tanker   
Bong-Gook Kang, Sang-Beom Shin, Dong-Hwan Park
Journal of Welding and Joining:79-86.  Publication Date (Web): February 27, 2014
PDF Links
 
37 A Study on Analyzing Thermal Strain of Weldment during Cooling used at Low MS Point Weld Consumables   
Yunsok Ha, Seongkil Nam, Sejin Park, Changgil Kwon
Journal of Welding and Joining:37-43.  Publication Date (Web): January 21, 2014
PDF Links
 
7 Verification of Validity of Governing Factors in High Accurate Prediction of Welding Distortion   
Jae-Yik Lee, Kyong-Ho Chang, You-Chul Kim
Journal of Welding and Joining:7-14.  Publication Date (Web): November 5, 2013
PDF Links
 
63 The Weldability of the Dissimilar Magnesium Alloy Welded by Fiber Laser   
Jong-Do Kim, Young-Sik Kim, Mook-Keun Song, Jung-Han Lee
Journal of Welding and Joining:63-68.  Publication Date (Web): June 5, 2013   Cited by 1
PDF Links
 
126 A Study on Bead Geometry Prediction the GMA Fillet Welding using Genetic Algorithm   
Young-Su Kim, Ill-Soo Kim, Ji-Hye Lee, Sung-Myoung Jung, Jong-Pyo Lee, Min-Ho Park, Reenal Ritesh Chand
Journal of Welding and Joining:126-132.  Publication Date (Web): December 23, 2012   Cited by 1
PDF Links
 
67 Patterns and Characteristics of Fatigue Failure in Cruciform Fillet Weld Joint
Yong-Bok Lee, Joon-Ki Chung, Sang-Heup Park
Journal of Welding and Joining:67-72.  Publication Date (Web): September 12, 2011
PDF Links
 
41 A Experiment Study for Selection of Welding Condition of fillet Welded Structure
Hyun-Ho Na, Ill-Soo Kim, Ji-Sun Kim, Ji-Hye Lee
Journal of Welding and Joining:41-47.  Publication Date (Web): September 12, 2011
PDF Links
 
45 Chracteristics of Fatigue Failure according to Thickness of Material and Number of Passes in Cruciform Fillet Weld Zone
YongBok Lee
Journal of Welding and Joining:45-50.  Publication Date (Web): January 10, 2011
PDF Links
 
59 Effect of Distance and Restraint Degree between Fillet and Butt Weldment on Residual Stress Redistribution at each Weldment
Hyung-Kook Jin, Dong-Ju Lee, Sang-Beom Shin
Journal of Welding and Joining:59-64.  Publication Date (Web): August 2, 2010
PDF Links
 
38 On the Fillet Weld-Induced Deformation Control by Applying the Tensioning Method
Joo-Sung Lee, Cheul-Ho Kim
Journal of Welding and Joining:38-43.  Publication Date (Web): September 14, 2009
PDF Links
 
60 A Study on the Buckling in Fillet Welds of Sheets
Hwan-Su Chu, Sang-Myung Cho
Journal of Welding and Joining:60-66.  Publication Date (Web): July 6, 2009
PDF Links
 
97 A Study on the Fatigue Life Assessment for Load-carrying Fillet Welded Joints using Stress Intensity Factor
Myung-Hyun Kim, Sung-Won Kang, Hyoung-Rae Kim
Journal of Welding and Joining:97-102.  Publication Date (Web): January 13, 2009
PDF Links
 
44 Development of Multi-pass Welding Method for Lifting Lug by Robot Weaving
Young-Zoo Kim, Kang-Uk Kim, Suk-Hyoung Kim, Sung-Won Kang, Soo-Ho Kim
Journal of Welding and Joining:44-52.  Publication Date (Web): January 28, 2008
PDF Links
 
14 Fatigue Tests of Welded Joints and Comparison Study of Foreign Codes
Byeong-Choon Goo, Jai-Hoon Kim
Journal of Welding and Joining:14-23.  Publication Date (Web): March 26, 2007
PDF Links
 
29 A Study on the Selection of Fillet Weld Conditions by Considering the Tack Welds
Jun-Young Lee, Jae-Woong Kim, Cheol-Hee Kim
Journal of Welding and Joining:29-36.  Publication Date (Web): January 4, 2007
PDF Links
 
27 A Study on the Fatigue Strength Evaluation for Fillet Weldment including Stress Singularity using Structural Stress with Virtual Node Method
Chung-In Ha, Sung-Won Kang, Myung-Hyun Kim, Man-Soo Kim, Sang-Yong Sohn, Joo-Ho Heo
Journal of Welding and Joining:27-33.  Publication Date (Web): August 22, 2006
PDF Links
 
1 |
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.