Optimization of Disk Laser Welding Parameters in Pure Ti Using Taguchi Method
Byeong-Ju Jin, Min-Ho Park, Tae-Jong Yun et al.
J Weld Join. 2018;36(1):34-40.   Published online January 25, 2018
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Optimization of Laser Welding Parameters in Titanium Sheet Using Grey-Fuzzy Logic
Byeong-Ju Jin, Min-Ho Park, Tae-Jong Yun et al.
J Weld Join. 2017;35(6):59-66.   Published online November 16, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Effects of laser power on hardness and microstructure of the surface melting hardened SKD61 hot die steel using Yb:YAG disk laser
Kwang-Hyeon Lee, Seong-Won Choi, Chung-Yun Kang
J Weld Join. 2015;33(3):54-61.   Published online June 30, 2015
PDFPDF    
Effect of Coating Thickness on Microstructures and Tensile Properties in Yb:YAG Disk Laser Welds of Al-Si Coated Boron Steel
Wei-Ye Cao, Jong-Pan Kong, Yong-Nam Ahn, Cheol-Hee Kim, Chung-Yun Kang
J Weld Join. 2013;31(3):66-75.   Published online June 30, 2013
PDFPDF    
Effect of B Contents on Hardness Characteristic of Disk Laser Beam Welded CP Steels
Tae-Jun Park, Jung-Woo Yu, Junil Kang, Tae-kyo Han, Kwang-Keun Chin, Chung-Yun Kang
J Weld Join. 2011;29(1):107-114.   Published online March 4, 2011
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI