Advanced Search  
 JWJ Search

61 Anticorrosion Performance of FCAW Cladding with Regard to the Influence of Heat Input   
Manas Kumar Saha, Ajit Mondal, Ritesh Hazra, Santanu Das
Journal of Welding and Joining:61-69.  Publication Date (Web): October 10, 2018
                  PDF Links
 
19 Gas Metal Arc Lap Joining of Aluminium Alloys and Steel Sheets   
Atanu Das, Amitava De
Journal of Welding and Joining:19-26.  Publication Date (Web): October 22, 2018
                  PDF Links
 
12 A Study on the Effect of Wire Composition on Welding with Gap and Offset in Cold Metal Transfer (CMT) GMAW   
Md. R. U. Ahsan, Taehoon Kim, Duck bong Kim, Changwook Ji, Yeong-Do Park
Journal of Welding and Joining:12-18.  Publication Date (Web): October 23, 2018
                  PDF Links
 
1 Laser and Gas Metal Arc Based Dissimilar Joining of Automotive Aluminium Alloys and Steel Sheets - A Review   
Atanu Das, Hee-Seon Bang
Journal of Welding and Joining:1-11.  Publication Date (Web): October 26, 2018
                  PDF Links
 
65 Spatter Generation During Constant Voltage DC-AC Pulse Tandem Gas Metal Arc Welding Process   
Sanghoon Kang, Hee-seon Bang, Cheolhee Kim
Journal of Welding and Joining:65-71.  Publication Date (Web): June 25, 2018   Cited by 1
                  PDF Links
 
38 Characteristics of Sulfide Stress Cracking of High Strength Pipeline Steel Weld by Heat Input   
Byoung-Hyun Yoon
Journal of Welding and Joining:38-44.  Publication Date (Web): May 29, 2018
                  PDF Links
 
23 Parametric Study of STS 316L Deposition with Arc and Wire Additive Manufacturing   
Tae Hyun Lee, Minjung Kang, Je Hoon Oh, Dong-Hyuck Kam
Journal of Welding and Joining:23-30.  Publication Date (Web): May 24, 2018
                  PDF Links
 
74 A Study on the Algorithm for Determining Back Bead Generation in GMA Welding Using Deep Learning   
Min Seok Kim, Seung Min Shin, Dong Hyun Kim, Sehun Rhee
Journal of Welding and Joining:74-81.  Publication Date (Web): April 13, 2018
                  PDF Links
 
103 Cathode Spot Phenomena Observation by High Speed Camera in Variable Polarity Aluminum Arc Welding   
Jungho Cho, Huncheol Jung, Kyungbae Park, Junkyung Lee
Journal of Welding and Joining:103-107.  Publication Date (Web): February 26, 2018
                  PDF Links
 
90 A Study on the Estimation of Weld Quality Using the Thermal Images During Arc Welding   
Ju-Yong Park, Woo-Seong Kim
Journal of Welding and Joining:90-94.  Publication Date (Web): February 21, 2018
                  PDF Links
 
65 A Review on Optimizations of Welding Parameters in GMA Welding Process   
Ill-Soo Kim, Min-Ho Park
Journal of Welding and Joining:65-75.  Publication Date (Web): February 5, 2018   Cited by 1
                  PDF Links
 
96 Development of Welding Consumables for GMAW and FCAW   
Tae-Hoon Kim, Chul-Gyu Park
Journal of Welding and Joining:96-100.  Publication Date (Web): December 15, 2017
                  PDF Links
 
65 Effects of Fluoride in the Flux on Hydrogen Content in Weld Metal and Operating Behavior in FCAW-S   
Woong Kil, Myeong-jun Shin, Kook-soo Bang
Journal of Welding and Joining:65-70.  Publication Date (Web): September 13, 2017   Cited by 1
                  PDF Links
 
23 A Study of Characteristics of Vertical-up SMA Welding by Short Circuit Control   
Kyung-Hun Lee, Hoi-Soo Ryoo, Soong-Keun Hyun
Journal of Welding and Joining:23-28.  Publication Date (Web): September 13, 2017
                  PDF Links
 
82 In-situ Strain Measurement of Submerged Arc Welding Process Through Application of Electronic Speckle Pattern Interferometry   
Uwe Reisgen, Rahul Sharma
Journal of Welding and Joining:82-88.  Publication Date (Web): August 14, 2017
                  PDF Links
 
16 Research Trend of Laser Welding and Weldability of High Speed Dissimilar Laser Lap Welding for Titanium   
Su-Jin Lee, Eunjoon Chun, Jeong SUH
Journal of Welding and Joining:16-22.  Publication Date (Web): August 14, 2017
                  PDF Links
 
23 Effects of Brazing Current on Mechanical Properties of Gas Metal Arc Brazed Joint of 1000MPa Grade DP Steels   
Wook-Je Cho, Tae-Jin Yoon, Sung-Yun Kwak, Jae-Hyeong Lee, Chung-Yun Kang
Journal of Welding and Joining:23-29.  Publication Date (Web): April 28, 2017
                  PDF Links
 
16 Influence of Gas Metal Arc Welding Parameters on the Bead Properties in Automatic Cladding   
Mathieu TERNER, Tsend-Ayush BAYARSAIKHAN, Hyun-Uk Hong, Je-Hyun Lee
Journal of Welding and Joining:16-25.  Publication Date (Web): January 19, 2017
                  PDF Links
 
1 The Latest Technology Development Trends of Flux Cored Wire   
Hee-Dae Im, Chang-Hyun Choi, Jae-Heon Jung, Woong Kil
Journal of Welding and Joining:1-10.  Publication Date (Web): December 29, 2016
                  PDF Links
 
70 Microstructure and Mechanical Properties of Gas Metal Arc Brazed Joint of DP Steel with Cu-Si Filler Metal   
Wook-Je Cho, Tae-Jin Yoon, Sung-Yun Kwak, Jae-Hyeong Lee, Chung-Yun Kang
Journal of Welding and Joining:70-76.  Publication Date (Web): October 30, 2016
                  PDF Links
 
62 High Efficient Welding Technology of the Car Bodies   
Hwan Tae Kim, Sang Cheol Kil
Journal of Welding and Joining:62-66.  Publication Date (Web): August 23, 2016
                  PDF Links
 
40 Porosity Reduction during Gas Tungsten Arc-Gas Metal Arc Hybrid Welding of Zinc Coated Steel Sheets (I) - Effect of Preceding Gas Tungsten Arc   
Minjung Kang, Young-Nam Ahn, Cheolhee Kim
Journal of Welding and Joining:40-47.  Publication Date (Web): August 23, 2016   Cited by 1
                  PDF Links
 
7 Development of Structural Steel and Trend of Welding Technology   
Sung Jin Kim, Hong Chul Jeong
Journal of Welding and Joining:7-20.  Publication Date (Web): February 29, 2016   Cited by 2
                  PDF Links
 
49 Fatigue Life Prediction of Non-Load-Carrying Cruciform Welded Joint using Master S-N Curve based on Structural Stress Approach   
Si-Young Kwak
Journal of Welding and Joining:49-54.  Publication Date (Web): December 31, 2015
PDF Links
 
50 Development of Durability Enhancement Technology for Arc Weldings in Advanced High Strength Steel (AHSS) Chassis Parts   
Kwang Bok Lee, Seung Taik Oh
Journal of Welding and Joining:50-56.  Publication Date (Web): August 31, 2015   Cited by 4
PDF Links
 
68 A study of model for nitrogen permeation in TIG welding of super duplex stainless steel   
Jae-Hyoung Lee, Byong-Ho Jung, Sang-Myung Cho, Jae-Ho Jun
Journal of Welding and Joining:68-74.  Publication Date (Web): June 30, 2015
PDF Links
 
91 The characteristics of bead welding on steel with process parameter during the laser-arc hybrid welding(Ⅱ) - Effect of heat input parameters -   
Jond-Do Kim, Gi-Hoon Myung, In-Duck Park
Journal of Welding and Joining:91-96.  Publication Date (Web): April 30, 2015
PDF Links
 
85 The characteristics of bead welding on steel with process parameter during the laser-arc hybrid welding(Ⅰ) - Effect of flow rate of shield gas and distance between laser and arc -   
Jong-Do Kim, Gi-Hoon Myung, Moo-Keun Song, Jae-Hwan Oh, Jeong Suh
Journal of Welding and Joining:85-90.  Publication Date (Web): April 30, 2015   Cited by 1
PDF Links
 
32 Numerical analysis on the welding residual stress and fracture toughness of the heavy thick steel welded joints by welding processes   
HanSur Bang, HeeSeon Bang
Journal of Welding and Joining:32-39.  Publication Date (Web): April 30, 2015
PDF Links
 
23 Optimization of arc brazing process parameters for exhaust system parts using box-behnken design of experiment   
Yong Kim, Pyeong-Won Park, Ki-Young Park, Jin-Chul Ryu
Journal of Welding and Joining:23-31.  Publication Date (Web): April 30, 2015   Cited by 1
PDF Links
 
1 | 2 | 3 |
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.