Won-Ho Choi 1 Articles
56 Influence of Welding Parameters on Macrostructure and Mechanical Properties of Friction-Stir-Spot-Welded 5454-O Aluminum Alloy Sheets
Won-Ho Choi, Yong-Jai Kwon, Sung-Ook Yoon, Myoung-Soo Kang, Chang-Yong Lim, Jong-Dock Seo, Sung-Tae Hong, Dong-Hwan Park, Kwang-Hak Lee
Journal of Welding and Joining:56-64.  Publication Date (Web): January 20, 2012
PDF Links
 
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.