196 Resistance Spot Welding Characteristics of Mg Alloy Applying Current Waveform Control   
Dong-Soon Choi, In-Sung Hwang, Dong-Cheol Kim, Jae-Wook Ryu, Moon-Jin Kang
Journal of Welding and Joining:196-201.  Publication Date (Web): May 14, 2014
PDF Links
 
27 Electrode Life Test of Resistance Spot Welding on Mg Alloy Using Dome Type Electrode   
Dong-Soon Choi, In-Sung Hwan, Dong-Cheol Kim, Moon-Jin Kang
Journal of Welding and Joining:27-31.  Publication Date (Web): January 21, 2014   Cited by 2
PDF Links
 
49 Resistance Spot Welding Characteristics of Mg Alloy Using Process Tape   
Dong-Soon Choi, Dong-Cheol Kim, Moon-Jin Kang
Journal of Welding and Joining:49-53.  Publication Date (Web): June 30, 2013   Cited by 2
PDF Links
 
49 A Study on Characteristic of Fracture in Lap Joint Welded STS429L
Dong-soon Choi, Jae-seong Kim, Hyun-jae Kim, Bo-young Lee
Journal of Welding and Joining:49-54.  Publication Date (Web): November 16, 2009
PDF Links
 
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.